SCC can develop at hot spots, including where the heat tracing attaches to pipe
Caustic (574: 7.4.6.2.n)
where dew points corrosion often occurs
Overhead fractionation (574:7.4.6.2.b)
Potential for none or very few CMLs on a circuit
Olefin cold side, Anhydrous ammonia (570:5.6.2
Relatively uniform corrosion
Sulfidation, Sour Water (570:5.6.3)
Valves that should be inspected for thermal fatigue
Cat Reformer (570:5.10)