SCC can develop at hot spots, including where the heat tracing attaches to pipe
Caustic 574: 7.4.6.2.n
Where dew point corrosion often occurs
Overhead fractionation 574: 7.4.6.2.b
Potential for none or very few CMLs on circuit
Olefin cold side, Anhydrous ammonia 570: 5.6.2
Relatively uniform corrosion
Sulfidation, Sour water 570: 5.6.3
Valves that should be inspected for thermal fatigue
Cat Reformer 570: 5.10